Abstract:
Introduction
Glass-ionomer cements and resin-modified glass-ionomers could be optimal orthodontic adhesives if they can provide adequate bonding strength. The aim of this study was to compare the shear bond strength of two orthodontic adhesives: Fuji Ortho LC and Transbond XT.
Materials and Methods
In this in vitro study, 32 sound extracted premolars were divided into two equal groups (n = 16). Brackets were bonded with Fuji Ortho LC in group 1 and Transbond XT in group 2. After 72 hours their shear bond strengths were measured; then the samples were analyzed under a stereomicroscope at ×10 and debonding locations were scored using Adhesive Remnant Index. Data were analyzed with t-test (α = 0.05).
Results
The mean shear bond strength values in groups 1 and 2 were 7.73 and 16.79, respectively, with no significant difference (p value
Conclusion
The shear bond strength of Fuji Ortho LC was less than that of Transbond XT, but still in an acceptable range for orthodontic bonding.
Language:
Persian
Published:
Journal of Isfahan Dental School, Volume:13 Issue: 3, 2017
Pages:
264 to 270
magiran.com/p1735849  
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یک‌ساله به مبلغ 1,390,000ريال می‌توانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
  • حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران می‌شود.
  • پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانه‌های چاپی و دیجیتال را به کاربر نمی‌دهد.
In order to view content subscription is required

Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!