The Effect of Cooling Rate on the Solutionizing of IN718 Superalloy Produced via Selective Laser Melting (SLM) Method
Author(s):
Article Type:
Research/Original Article (بدون رتبه معتبر)
Abstract:
In the present study, IN718 super alloy was produced by selective laser melting (SLM) method and was imposed under solution heat treatment at temperature of 1040°C for 2 hours. Three different environments, such as water, air and furnaces were used to cool the samples after complete solution. The results of microstructural studies conducted by optical microscopy (OM) and field emission scanning electron microscopy (FESEM) showed that intermetallic precipitates were formed during the process, disappear after solution. In order to complete the FESEM results, X-Ray diffraction (XRD) test showed that in at all cooling rates, the only remaining phases of matrix are the austenite (γ) and carbides, which their locations are between the grains according to the microscopic images. This issue indicates the proper selection of solution parameters and proper execution of solution process. The micro hardness test showed that doing solution treatment to reduce the volume fraction or completely remove the secondary phase leads to decreased hardness. By increasing cooling rate, the hardness of samples was reduced, so that the hardness of sample chilled in 30 % water was reduced compared to the sample before the heat treatment.
Keywords:
Language:
English
Published:
Journal of Environmental Friendly Materials, Volume:3 Issue: 1, Winter-Spring 2019
Pages:
17 to 22
magiran.com/p2002450
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یکساله به مبلغ 1,390,000ريال میتوانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
- حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران میشود.
- پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانههای چاپی و دیجیتال را به کاربر نمیدهد.
In order to view content subscription is required
Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!