Experimental Investigation on the dissimilar laser weld joints between Inconel 625 Superalloy and AISI 430 Ferritic Stainless Steel
Author(s):
Article Type:
Research/Original Article (دارای رتبه معتبر)
Abstract:
Mechanical properties optimization of weldment such as tensile strength, microhardness and impact toughness are of prime importance in welding technology. The main aim of this research is to investigate the microstructural evolutions and also optimization of tensile strength in dissimilar laser welding between Inconel 625 superalloy and AISI 430 ferritic stainless steel. It was found from the microhardness measurements that the hardness is increased form AISI 430 base metal toward Inconel 625 superalloy. This can be attributed to the inherent higher hardness of Inconel 625 and formation of very fine structure and also fine precipitations in the weld metal which are distributed uniformly. Formation of very fine structure and precipitations is due to the rapid cooling rate of the weld metal during laser welding process. Design of experiment based on the response surface method was used in order to optimize the tensile strength of the weld joints. Three process parameters i. e. pulse duration, lamping current and also travel speed were chosen as the main parameters which are considerably affecting the tensile strength of the weld joint. It was found that the lamping current has a higher impact on the tensile strength of the weld joints.
Keywords:
Language:
English
Published:
Journal of advanced materials and processing, Volume:8 Issue: 1, Winter 2020
Pages:
3 to 19
magiran.com/p2188059
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یکساله به مبلغ 1,390,000ريال میتوانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
- حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران میشود.
- پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانههای چاپی و دیجیتال را به کاربر نمیدهد.
In order to view content subscription is required
Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!