On the microstrctral and machanical properties of similar TLP bonding of Inconel 600 superalloy sheet
Author(s):
Article Type:
Research/Original Article (دارای رتبه معتبر)
Abstract:
In this study, microstructural evaluation and mechanical properties of similar TLP bonded of Inconel 600 by using of BNi-2 interlayer were investigated. The bonding tests were carried out at 1050°C and 1100°C for 5-45 min which homogenization treatment was performed on the best of the bonded samples. Results showed that Ni-B eutectic compound was formed in the a-thermally solidification zone (ASZ) of the bonded sample at 1050°C. In addition to existence of the Ni-B compound, Cr-B was observed in the ASZ of the bonded sample at 1100°C. Ni-B and Ni-Cr-B were formed in the diffusion affected zone (DAZ). TLP bonded sample at 1050°C for 45min including discontinuous areas of ASZ in isothermal solidification zone (ISZ) was the best bonded sample. Homogenization process was carried out on this sample caused to elimination of the eutectic compounds, completely. Mechanical investigation revealed that due to existence of the intermetallic compounds in the ASZ and DAZ, value of hardness for this region were about 510 and 311 HV, respectively. Whit elimination of the intermetallic compounds by performing of homogenization treatment, mechanical properties of the boding region were improved.
Keywords:
Language:
Persian
Published:
Journal of Welding Science and Technology of Iran, Volume:3 Issue: 2, 2018
Pages:
90 to 104
https://magiran.com/p1796047
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یکساله به مبلغ 1,390,000ريال میتوانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
- حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران میشود.
- پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانههای چاپی و دیجیتال را به کاربر نمیدهد.
In order to view content subscription is required
Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!